Decison 8/2024 - Adoption of NWI EN ISO 16573-1 Steel — Measurement method for the evaluation of hydrogen embrittlement resistance of high strength steels — Part 1: Constant load test

Scope

This document provides a method for the evaluation of the resistance to hydrogen embrittlement (i.e. hydrogen delayed fracture) using constant loading test with hydrogen precharged specimens.

Purpose

CEN/TC 459/SC 1 members agreed to register in the work program the following standards as EN ISO. The projects are developed under Vienna Agreement with ISO lead.

Comment on proposal

Required form fields are indicated by an asterisk (*) character.


Please email further comments to: debbie.stead@bsigroup.com

Follow standard

You are now following this standard. Weekly digest emails will be sent to update you on the following activities:

You can manage your follow preferences from your Account. Please check your mailbox junk folder if you don't receive the weekly email.

Unfollow standard

You have successfully unsubscribed from weekly updates for this standard.

Error